PML
|
Use |
VLT
|
UV cut
|
Rfvis
|
TSER
|
Quality
|
Thickness |
TAIZHEN 70 | Before the window | 72% | ≥99% | 12% | 60% | 10 | 3mil |
TAIZHEN 25+ | Lientang window | 22% | ≥99% | 6% | 69% | 10 | 3mil |
TAIZHEN 25 | Lientang window | 31% | ≥99% | 13% | 54% | 10 | 2mil |
TAIZHEN 15 | Lientang window | 15% | ≥99% | 20% | 69% | 10 | 2mil |
TAIZHEN 70v |
Before the window |
70% |
≥99% |
11% |
58% | 8 | 3mil |
TAIZHEN 25v |
Lientang window |
28% |
≥99% |
10% | 64% | 8 | 3mil |
PML | Use |
VLT |
UV cut |
TAIZHEN 70 | Before the window | 72% | ≥99% |
TAIZHEN 25+ | Lientan gwindow | 22% | ≥99% |
TAIZHEN 25 | Lientan gwindow | 31% | ≥99% |
TAIZHEN 15 | Lientan gwindow | 15% | ≥99% |
PML |
Rfvis |
TSER
|
Quality
|
Thickness |
TAIZHEN 70 |
12% |
60% | 10 | 3mil |
TAIZHEN 25+ |
6% |
69% | 10 | 3mil |
TAIZHEN 25 |
13% |
54% | 10 | 2mil |
TAIZHEN 15 |
20% |
69% | 10 | 2mil |
PML |
Use |
VLT |
UV cut
|
Rfvis
|
TSER
|
Quality
|
Thickness |
HENGXIN 75 | Before the window | 72% | ≥99% | 12% | 38% | 5 | 2mil |
HENGXIN 30 | Lientang window | 33% | ≥99% | 8% | 44% | 5 | 2mil |
HENGXIN 15 | Lientang window | 18% | ≥99% | 8% | 47% | 5 | 2mil |
PML |
Use |
VLT |
UV cut |
HENGXIN 75 | Before the window | 72% | ≥99% |
HENGXIN 30 | Lientang window | 33% | ≥99% |
HENGXIN 15 | Lientang window | 18% | ≥99% |
PML |
Rfvis |
TSER
|
Quality
|
Thickness |
HENGXIN 75 |
12% | 38% | 5 | 2mil |
HENGXIN 30 |
8% | 44% | 5 | 2mil |
HENGXIN 15 |
8% | 47% | 5 | 2mil |
PML |
Use |
VLT
|
UV cut
|
Rfvis
|
TSER
|
Quality
|
Thickness |
BINGCUI 70 | Before the window | 72% | ≥99% | 11% | 47% | 8 | 2mil |
BINGCUI 30 | Lientang window | 32% | ≥99% | 6% | 53% | 8 | 2mil |
BINGCUI 15 | Lientang window | 16% | ≥99% | 6% | 62% | 8 | 2mil |
BINGCUI 70+ |
Before the window |
70% |
≥99% |
10% | 51% | 8 | 4mil |
BINGCUI 20+ |
Lientang window |
22% |
≥99% |
8.4% | 62% | 8 | 4mil |
PML |
Use |
VLT |
UV cut |
BINGCUI 70 | Before the window | 72% | ≥99% |
BINGCUI 30 | Lientang window | 32% | ≥99% |
BINGCUI 15 | Lientang window | 16% | ≥99% |
PML |
Rfvis |
TSER
|
Quality
|
Thickness |
BINGCUI 70 |
11% | 47% | 8 | 2mil |
BINGCUI 30 |
6% | 53% | 8 | 2mil |
BINGCUI 15 |
6% | 62% | 8 | 2mil |
Tensile range increase of 31%
Craping self-healing performance improved by 42%
Shock prevent penetrate performance increase 35%
Fouling rain spot resistance increase of 50%
Aging resistance to yellowing resistance capacity increase of 38%
The installation process performance increase of 30%
Thickness | Repair function | Anti-fouling level |
High and low temperature resistance |
Original factory warranty |
6.5mil | Hot repair | Good | -35℃——116℃ | 5 Years |
Thickness | Repair function |
Anti-fouling level |
High and low temperature resistance |
Original factory warranty |
7.5mil | Hot repair | Good | -35℃——116℃ | 10 Years |
Thickness | Repair function |
Anti-fouling level |
7.5mil | Hot repair | Good |
High and low temperature resistance |
Original factory warranty |
-35℃——116℃ | 10 Years |
Thickness | Repair function |
Anti-fouling level |
High and low temperature resistance |
Original factory warranty |
7.5mil | Hot repair | Good | -35℃——116℃ | 8 Years |
Thickness | Repair function |
Anti-fouling level |
7.5mil | Hot repair | Good |
High and low temperature resistance |
Original factory warranty |
-35℃——116℃ | 8 Years |